Electrochemical extraction, refining of metals and their uses
Use ΔG° = −nFE° to judge displacement reactions, explain the Hall-Héroult process, describe distillation, liquation, electrolytic, zone and vapour-phase refining, and list uses of Al, Zn, Fe, Cu and Au.
If something looks wrong, please tell us.
By the end of this lesson you can
- Use ΔG° = −nFE° to decide whether a metal displaces another from solution.
- Write the electrode reactions of the Hall-Héroult process and calculate the charge needed.
- Explain each refining method and name a metal refined by it.
- List important uses of aluminium, zinc, iron, copper and gold.
Carbon cannot reduce the oxides of very reactive metals such as sodium, potassium and aluminium at a practical temperature. These metals are extracted by electrochemical methods, from a fused salt or a solution, either by electrolysis or by a more reactive metal. The crude metal from any method is then refined.
The electrochemical principle
ΔG° = −nFE°, where n = electrons transferred, F = 96,485 C mol⁻¹ (the faraday), E° = standard emf of the cell reaction.
If E° is positive, ΔG° is negative and the reaction is spontaneous. So a more reactive metal placed in a solution of the ions of a less reactive metal goes into solution and the less reactive metal is deposited: Cu(s) + 2Ag⁺(aq) → Cu²⁺(aq) + 2Ag(s), and Zn(s) + Cu²⁺(aq) → Zn²⁺(aq) + Cu(s).
Worked example 1: will the displacement happen?
Standard reduction potentials: Ag⁺/Ag = +0.80 V; Cu²⁺/Cu = +0.34 V; Zn²⁺/Zn = −0.76 V. (a) Zn + Cu²⁺: E° = E°(cathode, Cu) − E°(anode, Zn) = 0.34 − (−0.76) = +1.10 V; ΔG° = −2 × 96,485 × 1.10 = −212,267 J ≈ −212 kJ: feasible. (b) Cu + 2Ag⁺: E° = 0.80 − 0.34 = +0.46 V; ΔG° = −2 × 96,485 × 0.46 = −88,766 J ≈ −88.8 kJ: feasible. (c) Cu + Zn²⁺: E° = −0.76 − 0.34 = −1.10 V, ΔG° = +212 kJ: not feasible; copper cannot displace zinc.
Hall-Héroult process for aluminium
Electrolysis is done in an iron tank lined with carbon, which is the cathode; carbon blocks dipping into the melt are the anodes. The electrolyte is a solution of pure alumina (about 20%, according to the textbook) in molten cryolite (Na₃AlF₆), with about 10% calcium chloride added. Cryolite and CaCl₂ lower the melting point of the mixture and make it conduct; the melt is kept above 1270 K.
- Ionisation: Al₂O₃ → 2Al³⁺ + 3O²⁻
- Cathode: 2Al³⁺(melt) + 6e⁻ → 2Al(l)
- Anode: 6O²⁻(melt) → 3O₂ + 12e⁻; the hot carbon anode also reacts: C(s) + O²⁻ → CO + 2e⁻ and C(s) + 2O²⁻ → CO₂ + 4e⁻
- Net: 4Al³⁺(melt) + 6O²⁻(melt) + 3C(s) → 4Al(l) + 3CO₂(g) (check: Al 4; O 6 = 3 × 2; C 3; charge +12 − 12 = 0)
Because the anode carbon is burnt to CO and CO₂, the anodes are slowly used up and must be replaced. Molten aluminium collects at the bottom of the cell.
Worked example 2: charge for 1 kg of aluminium
Use Al = 27.0 g mol⁻¹ and F = 96,485 C mol⁻¹. Working: moles of Al = 1000 ÷ 27.0 = 37.04 mol. Each Al³⁺ needs 3 e⁻, so moles of electrons = 3 × 37.04 = 111.1 mol. Charge Q = 111.1 × 96,485 = 1.07 × 10⁷ C. Carbon burnt (net equation, 3C per 4Al) = 37.04 × 3/4 = 27.78 mol = 27.78 × 12.0 = 333 g of anode per kilogram of aluminium.
Refining the crude metal
Crude metal contains unreacted ore, other metals and non-metals. Removing them is refining. The method depends on the metal and its impurities.
- Distillation: for low-boiling metals such as zinc (b.p. 1180 K) and mercury (630 K). The impure metal is evaporated and the vapour condensed.
- Liquation: for low-melting metals such as tin (m.p. 904 K), lead (600 K), mercury (234 K) and bismuth (545 K) carrying high-melting impurities. The crude metal is heated just above its melting point on the sloping hearth of a reverberatory furnace, without air; the pure metal flows down, the impurities stay behind.
- Electrolytic refining: impure metal is the anode, a thin strip of pure metal is the cathode, and the electrolyte is a solution of a salt of the metal. For silver: electrolyte acidified AgNO₃; anode Ag(s) → Ag⁺(aq) + e⁻; cathode Ag⁺(aq) + e⁻ → Ag(s). Less electropositive impurities fall below the anode as anode mud. Copper and zinc are refined similarly.
- Zone refining: based on fractional crystallisation; impurities are more soluble in the melt than in the solid. A heater moves slowly along a rod of the metal, melting a narrow zone; pure metal crystallises behind it and the impurities travel with the molten zone to one end. Repeated several times in an inert gas, it gives the ultrapure germanium, silicon and gallium used in semiconductors.
- Vapour-phase refining: the metal forms a volatile compound that is then decomposed to the pure metal. The basic requirements: the metal must form a volatile compound with an available reagent, and that compound must decompose easily to give back the metal.
Two vapour-phase methods
Mond process (nickel): impure nickel heated in CO at about 350 K forms volatile nickel tetracarbonyl, Ni(s) + 4CO(g) → [Ni(CO)₄](g), leaving solid impurities behind; at about 460 K the carbonyl decomposes, [Ni(CO)₄](g) → Ni(s) + 4CO(g). Van Arkel method (titanium, zirconium): the impure metal is heated with iodine in an evacuated vessel at about 550 K, Ti(s) + 2I₂(s) → TiI₄(vapour); the vapour passes over a tungsten filament at about 1800 K, where TiI₄ → Ti(s) + 2I₂, depositing pure titanium; the iodine is reused.
Refining methods and the metals they suit
-
Distillation
- Volatile metals
- Zn, Hg
-
Liquation
- Low-melting metals
- Sn, Pb, Hg, Bi
-
Electrolytic refining
- Impure anode, pure cathode
- Ag, Cu, Zn
-
Zone refining
- Ultrapure semiconductors
- Ge, Si, Ga
-
Vapour phase
- Mond: Ni
- Van Arkel: Ti, Zr
Uses of some metals
| Metal | Important uses (from the Tamil Nadu textbook) |
|---|---|
| Aluminium | Cooking vessels, heat exchangers and sinks; foil for packing food; light strong alloys (with Cu, Mn, Mg, Si) for aircraft; chemical reactors, medical equipment, refrigeration units, gas pipelines; overhead cables with a steel core |
| Zinc | Galvanising iron and steel; die-castings; ZnO in paints, rubber, cosmetics, medicines, plastics, inks and batteries; ZnS in luminous paints, fluorescent lights and X-ray screens; brass for water valves |
| Iron | Bridges, pylons, bicycle chains, tools; cast iron pipes, valves and stoves; magnets; stainless steel cutlery and surgical instruments; nickel steel for cables and aircraft parts; chrome steel for cutting tools |
| Copper | The first metal used by humans (its alloy bronze gave the Bronze Age); coins and ornaments; wires, water pipes and electrical parts |
| Gold | Coinage and jewellery (alloyed with copper); electroplating of watches, electrical connectors and dental work; gold nanoparticles as catalysts and in solar cells |
The textbook also describes the iron pillar in Delhi, about 1600 years old, which has resisted rusting because a thin protective layer (misawite, a compound of iron, oxygen and hydrogen) formed on it.
Key takeaways: positive E° means negative ΔG° and a feasible reduction. In the Hall-Héroult cell Al³⁺ is reduced at the carbon-lined cathode and the carbon anodes burn away. Refining: distil volatile metals, liquate low-melting ones, electrolyse with an impure anode, zone-refine semiconductors, and use volatile compounds for Ni (Mond) and Ti or Zr (Van Arkel).
Check your understanding
-
1. Which reaction is NOT feasible under standard conditions? (E°: Zn²⁺/Zn −0.76 V, Fe²⁺/Fe −0.44 V, Cu²⁺/Cu +0.34 V, Ag⁺/Ag +0.80 V)
- Zn + Cu²⁺ → Cu + Zn²⁺
- Cu + Zn²⁺ → Zn + Cu²⁺
- Cu + 2Ag⁺ → 2Ag + Cu²⁺
- Fe + Cu²⁺ → Cu + Fe²⁺
Show answer
Answer: B. For Cu + Zn²⁺, E° = E°(Zn²⁺/Zn) − E°(Cu²⁺/Cu) = −0.76 − 0.34 = −1.10 V. A negative E° makes ΔG° = −nFE° positive, so copper cannot displace zinc. The other three have positive E° (1.10, 0.46 and 0.78 V).
-
2. In the Hall-Héroult process, cryolite is added mainly to
- remove impurities from alumina
- act as the anode
- lower the melting point of alumina and make the melt conduct
- reduce Al³⁺ chemically
Show answer
Answer: C. Pure alumina melts at a very high temperature. Dissolving it in molten cryolite (with some CaCl₂) gives a melt that can be worked at about 1270 K and conducts electricity.
-
3. In the electrolytic refining of copper, the anode is
- impure copper
- pure copper
- a carbon rod
- a platinum electrode
Show answer
Answer: A. The impure metal is made the anode so that copper dissolves from it; pure copper deposits on the pure-copper cathode, and less electropositive impurities collect as anode mud.
-
4. Zr(impure) + 2I₂ → ZrI₄ at about 523 K, then ZrI₄ → Zr(pure) + 2I₂ at about 1800 K. This method is
- the Mond process
- zone refining
- liquation
- the Van Arkel method
Show answer
Answer: D. Forming a volatile tetraiodide and decomposing it on a hot tungsten filament is the Van Arkel method, used for Zr and Ti. The Mond process uses CO to refine nickel.
-
5. How many coulombs are needed to deposit 10.8 g of silver from Ag⁺ during electrolytic refining? (Ag = 108 g mol⁻¹, F = 96,485 C mol⁻¹)
- 96,485 C
- 9,648.5 C
- 19,297 C
- 1,042 C
Show answer
Answer: B. Moles of Ag = 10.8 ÷ 108 = 0.100 mol. Ag⁺ + e⁻ → Ag needs 1 mol electrons per mol Ag, so 0.100 mol e⁻. Q = 0.100 × 96,485 = 9,648.5 C.