• Practice
  • About 22 min
  • 5 practice questions

Minerals, ores and the concentration of ores

Tell a mineral from an ore, name the common ores of important metals, list the three main stages of metallurgy and choose gravity separation, froth flotation or magnetic separation for a given ore.

If something looks wrong, please tell us.

By the end of this lesson you can

  • Explain why a few metals occur native while most occur combined.
  • Tell a mineral from an ore and give examples.
  • List the three stages of extracting a metal from its ore.
  • Explain gravity separation, froth flotation (with collectors and depressants) and magnetic separation, and pick the right one for an ore.

Metallurgy is the science and technology of metals: how they are taken out of the earth, purified and used. Our cooking vessels, electric wires, bicycles and coins all depend on it. This unit of the Tamil Nadu textbook follows a metal from the mine to the pure metal, and explains the chemistry behind every step.

How metals occur in nature

Metals that react very little, such as copper, silver, gold and platinum, can be found in significant amounts as the free element: they occur native. Reactive metals, such as the alkali metals, are always found combined, as oxides, sulphides, carbonates, silicates, halides and so on, and must be extracted chemically.

Mineral and ore

A mineral is a naturally occurring substance obtained by mining that contains a metal, either free or as a compound. An ore is a mineral that contains a high enough percentage of the metal for the metal to be extracted conveniently and economically. So every ore is a mineral, but not every mineral is an ore.

Aluminium is the classic example. Both bauxite (Al₂O₃·nH₂O) and china clay (kaolinite, Al₂Si₂O₅(OH)₄) contain aluminium, but only bauxite is worth processing; getting aluminium out of clay is not profitable. Bauxite is therefore an ore of aluminium, china clay is not. Likewise iron occurs in hundreds of minerals, but haematite and magnetite are the ones used.

Common ores, as listed in the Tamil Nadu textbook (table 1.1)
MetalOre (formula)
AluminiumBauxite Al₂O₃·nH₂O; diaspore Al₂O₃·H₂O; kaolinite Al₂Si₂O₅(OH)₄
IronHaematite Fe₂O₃; magnetite Fe₃O₄; siderite FeCO₃; iron pyrite FeS₂; limonite Fe₂O₃·3H₂O
CopperCopper pyrite CuFeS₂; copper glance Cu₂S; cuprite Cu₂O; malachite CuCO₃·Cu(OH)₂; azurite 2CuCO₃·Cu(OH)₂
ZincZinc blende (sphalerite) ZnS; calamine ZnCO₃; zincite ZnO
LeadGalena PbS; anglesite PbSO₄; cerussite PbCO₃
TinCassiterite (tin stone) SnO₂
SilverSilver glance (argentite) Ag₂S; horn silver (chlorargyrite) AgCl; ruby silver (pyrargyrite) Ag₃SbS₃

Worked example 1: how much metal does an ore hold?

Compare haematite and magnetite as iron ores. Use Fe = 55.85 and O = 16.00. Working: Fe₂O₃ has molar mass 2 × 55.85 + 3 × 16.00 = 111.70 + 48.00 = 159.70 g mol⁻¹, so % Fe = 111.70 ÷ 159.70 × 100 = 69.9%. Fe₃O₄ has molar mass 3 × 55.85 + 4 × 16.00 = 167.55 + 64.00 = 231.55 g mol⁻¹, so % Fe = 167.55 ÷ 231.55 × 100 = 72.4%. Both are rich in iron, which is one reason they are ores. (A real ore also contains rock, so the actual iron content of a mined lump is lower.)

The three stages of metallurgy

From ore to pure metal

  1. Concentration of the ore Remove gangue (rock, sand, earthy matter) so the metal compound is enriched.
  2. Extraction of crude metal Convert the ore to the oxide, then reduce the oxide to the metal.
  3. Refining of crude metal Remove the remaining impurities to get pure metal.

Concentration of ores

Mined ore is mixed with non-metallic impurities, rocky material and siliceous matter, together called gangue. Removing gangue is concentration (also called ore dressing). The method chosen depends on the nature of the ore, the kind of impurity and environmental factors.

Gravity separation (hydraulic washing)

Used when the ore particles are much heavier (higher specific gravity) than the gangue. The finely powdered ore is treated with a fast current of water; the light gangue is washed away and the heavy ore settles. It suits native gold and heavy oxide ores such as haematite (Fe₂O₃) and tin stone (SnO₂).

Froth flotation

Used for sulphide ores such as galena (PbS) and zinc blende (ZnS). It works because sulphide particles are wetted preferentially by oil, while gangue is wetted by water.

  1. The crushed ore is suspended in water with a frothing agent such as pine oil or eucalyptus oil.
  2. A little sodium ethyl xanthate is added as a collector: it attaches to the ore particles and makes them water-repellent.
  3. Air is blown through the mixture to make a froth. Oil-wetted ore particles rise with the froth; it is skimmed off and dried.
  4. Water-wetted gangue particles sink to the bottom.

If the ore holds a second metal sulphide as an impurity, a depressant such as sodium cyanide or sodium carbonate keeps that sulphide out of the froth. In galena containing ZnS, NaCN forms a layer of the complex Na₂[Zn(CN)₄] on the zinc sulphide surface, so ZnS stays in the water while PbS floats.

Magnetic separation

Used when the ore and the impurity differ in magnetic behaviour. The crushed ore falls on a belt moving over two rollers, one of them magnetic. Magnetic particles cling to the magnetic roller and drop in a heap close to it; non-magnetic particles fly off farther away. Tin stone (non-magnetic) is freed from magnetic wolframite this way, and magnetic ores such as chromite and pyrolusite are separated from non-magnetic siliceous gangue.

Choosing a physical concentration method

  • Gravity separation
    • Property used: density
    • Ore heavier than gangue
    • Gold, haematite, tin stone
  • Froth flotation
    • Property used: wetting by oil
    • Sulphide ores
    • Galena, zinc blende; NaCN depresses ZnS
  • Magnetic separation
    • Property used: magnetism
    • Ore or impurity is magnetic
    • Tin stone from wolframite; chromite

Worked example 2: choosing the method

A sample of galena contains some zinc blende and sand. Which method, and what extra reagent? Working: galena is a sulphide, so froth flotation is used (pine oil as frother, sodium ethyl xanthate as collector). Zinc blende is also a sulphide and would float too, so sodium cyanide is added as a depressant; it coats ZnS with Na₂[Zn(CN)₄] and holds it back. Sand is wetted by water and sinks.

Gangue + ore → concentration. Heavy ore: gravity. Sulphide ore: froth flotation. Magnetic difference: magnetic separation. Chemical solubility: leaching (next lesson).

Key takeaways: all ores are minerals but not all minerals are ores; the deciding test is economic extraction. Metallurgy runs concentration → extraction → refining. Physical concentration uses density, oil-wetting or magnetism.

Check your understanding

  1. 1. Why is bauxite an ore of aluminium while china clay is not?

    1. China clay contains no aluminium.
    2. Aluminium can be extracted from bauxite conveniently and economically, but not from china clay.
    3. Bauxite is a sulphide and china clay is an oxide.
    4. China clay is not a mineral.
    Show answer

    Answer: B. China clay (Al₂Si₂O₅(OH)₄) does contain aluminium and is a mineral, so options one and four are wrong; neither is a sulphide. The difference is economic: aluminium is profitably extracted only from bauxite, which is what makes a mineral an ore.

  2. 2. Which ore is best concentrated by froth flotation?

    1. Haematite
    2. Cassiterite
    3. Galena
    4. Magnetite
    Show answer

    Answer: C. Froth flotation suits sulphide ores. Galena is PbS. Haematite (Fe₂O₃), cassiterite (SnO₂) and magnetite (Fe₃O₄) are oxides, concentrated by gravity or magnetic methods.

  3. 3. In froth flotation, what does sodium ethyl xanthate do?

    1. It produces the froth.
    2. It depresses zinc sulphide.
    3. It dissolves the gangue.
    4. It acts as a collector, making ore particles water-repellent.
    Show answer

    Answer: D. The frothing agent is pine or eucalyptus oil. Sodium ethyl xanthate is the collector: it attaches to sulphide particles and makes them water-repellent so they rise with the froth. Sodium cyanide is the depressant for ZnS.

  4. 4. Tin stone is freed from wolframite by

    1. magnetic separation
    2. froth flotation
    3. calcination
    4. smelting
    Show answer

    Answer: A. Wolframite is magnetic and tin stone is not, so an electromagnetic separator divides them. Froth flotation is for sulphides; calcination and smelting are not concentration methods.

  5. 5. What is the percentage of copper in copper glance, Cu₂S? (Cu = 63.55, S = 32.07)

    1. 34.6%
    2. 66.5%
    3. 88.8%
    4. 79.9%
    Show answer

    Answer: D. Molar mass of Cu₂S = 2 × 63.55 + 32.07 = 127.10 + 32.07 = 159.17 g mol⁻¹. % Cu = 127.10 ÷ 159.17 × 100 = 79.9%. (34.6% is the copper content of CuFeS₂.)

Sign in to keep track of the lessons you finish.

Next lesson → Leaching, roasting and calcination

Privacy · Terms · Refunds · Delivery