Rubber, molecular mass of polymers and biodegradable polymers

Describe natural rubber and vulcanisation, calculate number-average and weight-average molar masses, and name common biodegradable polymers.

If something looks wrong, please tell us.

This lesson finishes the course with three ideas that appear together in most syllabuses: what makes rubber elastic and how vulcanisation improves it, how chemists describe the molar mass of a polymer whose chains have different lengths, and which polymers can be broken down by living organisms.

Natural rubber

Natural rubber is cis-1,4-polyisoprene, made of isoprene units. The cis arrangement around each double bond bends the chain, so the chains are coiled and held only by weak van der Waals forces. When stretched, they uncoil; when released, they coil up again. The trans form of the same polymer, gutta-percha, packs more closely and is hard rather than elastic.

Vulcanisation

Raw natural rubber becomes soft and sticky when warm and brittle when cold, and it absorbs a lot of water. Vulcanisation removes these faults: the rubber is heated with sulphur (with an additive to speed it up). Sulphur forms cross-links between chains at the reactive positions next to the double bonds. The cross-links stop the chains from sliding permanently, so vulcanised rubber is harder, stronger and keeps its elasticity over a wider range of temperature. More sulphur gives a harder product. Neoprene, a synthetic rubber, is the polymer of chloroprene (2-chloro-1,3-butadiene) and resists oils and heat better.

Molar mass of a polymer

A polymer sample has chains of many lengths, so its molar mass is an average. Two averages are used. The number-average molar mass counts every molecule equally: Mn = ΣNiMi ÷ ΣNi, where Ni molecules have molar mass Mi. The weight-average molar mass gives heavier molecules more weight: Mw = ΣNiMi^2 ÷ ΣNiMi. The ratio PDI = Mw ÷ Mn is the polydispersity index. It is never less than 1, and equals 1 only when all chains are the same length, which is close to true for many natural polymers such as proteins. Synthetic polymers usually have PDI greater than 1.

Worked example 1: averages from numbers of molecules

A sample has 10 molecules of molar mass 10 000 g/mol and 10 molecules of 20 000 g/mol. Mn = (10 × 10 000 + 10 × 20 000) ÷ 20 = 300 000 ÷ 20 = 15 000 g/mol. Mw = (10 × 10 000^2 + 10 × 20 000^2) ÷ (10 × 10 000 + 10 × 20 000) = (1 × 10^9 + 4 × 10^9) ÷ (3 × 10^5) = 5 × 10^9 ÷ 3 × 10^5 ≈ 16 667 g/mol. PDI = 16 667 ÷ 15 000 ≈ 1.11.

Worked example 2: averages from masses

A sample is half by mass chains of 10 000 g/mol and half by mass chains of 30 000 g/mol. When mass fractions w are given, Mw = Σw_iM_i = 0.5 × 10 000 + 0.5 × 30 000 = 20 000 g/mol, and Mn = 1 ÷ Σ(w_i ÷ M_i) = 1 ÷ (0.5 ÷ 10 000 + 0.5 ÷ 30 000) = 1 ÷ (6.667 × 10^−5) = 15 000 g/mol. PDI = 20 000 ÷ 15 000 = 1.33. Check: 1 g of sample holds 0.5 ÷ 10 000 + 0.5 ÷ 30 000 mol of chains, so the average mass per mole is indeed 15 000 g.

Biodegradable polymers

Most synthetic polymers resist breakdown and persist as waste. Biodegradable polymers contain groups, often ester or amide links, that microorganisms can break. Two textbook examples: PHBV (poly-β-hydroxybutyrate-co-β-hydroxyvalerate), a copolymer of 3-hydroxybutanoic acid and 3-hydroxypentanoic acid, used in packaging and in some medical items; and nylon-2–nylon-6, an alternating polyamide of glycine and aminocaproic acid.

Mn = ΣNiMi ÷ ΣNi; Mw = ΣNiMi^2 ÷ ΣNiMi; PDI = Mw ÷ Mn ≥ 1. Vulcanisation = heating rubber with sulphur to form cross-links.

Key takeaways: natural rubber is elastic because its cis chains are coiled and weakly held; sulphur cross-links make it tougher; Mw is always at least Mn because heavy chains count more; and biodegradable polymers such as PHBV and nylon-2–nylon-6 carry links that microorganisms can break.

Check your understanding

  1. 1. Vulcanisation of rubber introduces

    1. oxygen bridges between chains
    2. hydrogen bonds between chains
    3. sulphur cross-links between chains
    4. benzene rings into the chain
    Show answer

    Answer: C. Heating rubber with sulphur forms sulphur cross-links between chains, making it harder and less sticky.

  2. 2. Natural rubber is

    1. cis-1,4-polyisoprene
    2. trans-1,4-polyisoprene
    3. polychloroprene
    4. polystyrene
    Show answer

    Answer: A. Natural rubber has the cis arrangement; the trans form is gutta-percha. Polychloroprene is neoprene.

  3. 3. A sample has 5 molecules of molar mass 20 000 g/mol and 5 of 40 000 g/mol. Its number-average molar mass is

    1. 25 000 g/mol
    2. 33 333 g/mol
    3. 60 000 g/mol
    4. 30 000 g/mol
    Show answer

    Answer: D. Mn = (5 × 20 000 + 5 × 40 000) ÷ 10 = 300 000 ÷ 10 = 30 000 g/mol.

  4. 4. The polydispersity index of a polymer sample is

    1. always less than 1
    2. always equal to or greater than 1
    3. always exactly 2
    4. negative for synthetic polymers
    Show answer

    Answer: B. PDI = Mw ÷ Mn, and Mw is never smaller than Mn, so PDI ≥ 1. It equals 1 only when all chains have the same length.

  5. 5. Which of these is a biodegradable polymer?

    1. PVC
    2. Polystyrene
    3. PHBV
    4. Teflon
    Show answer

    Answer: C. PHBV, a copolymer of 3-hydroxybutanoic and 3-hydroxypentanoic acids, is broken down by microorganisms. The others persist in the environment.